06-14-2008, 15:49
I need some advice...
What is the best way to polish my handmade flat glass to cerium/mirror finish? One side is frosted from the contact with the kiln wash during the fabrication...
I am planning the following:
120-240-400 on the lap
600-800-1200-1800 against float glass
Then cerium oxide buffing.
Would that work?
What is the best way to polish my handmade flat glass to cerium/mirror finish? One side is frosted from the contact with the kiln wash during the fabrication...